摘要

应用于口腔修复领域的材料主要是陶瓷类材料,其发展经过了一个漫长的过程。氧化锆类陶瓷材料,因其出色的机械性能以及美学性能,是目前口腔医生应用于临床最多的一种修复体。有学者在氧化锆材料的基础上发现了新型纳米氧化锆,并声称其具有更加出色的性能。目前已有学者通过研究发现氧化锆陶瓷在长期使用后会使材料变脆,导致其疲劳失效,但研究大都局限于干燥环境下,而口腔主要为复杂的湿润环境。本文对口腔陶瓷类材料发展史进行总结概述,并探讨干湿环境下氧化锆陶瓷的循环疲劳性能的可能研究方向。

关键词: 氧化锆;发展史;唾液;循环加载

Abstract

The materials used in the field of prosthodontics are mainly ceramic materials, and its development has gone through a long process. Zirconia ceramic materials, due to their excellent mechanical and aesthetic properties, are the most widely used prosthetics in clinic by dentists. Some scholars have found a new type of nano zirconia based on zirconia materials and claimed that it has better properties. At present, scholars have found that zirconia ceramics will make the material brittle and lead to fatigue failure after long-term use, but most of the research is limited to the dry environment, and the oral cavity is mainly a complex humid environment. This paper summarizes the development history of dental ceramics, and discusses the possible research direction of cyclic fatigue properties of zirconia ceramics in dry and wet environment.

Key words: Zirconia; Development history; Saliva; Cyclic loading

参考文献 References

[1] AZA A H D, CHEVALIER J, FANTOZZI G, et al. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses[J]. Biomaterials, 2002, 23(3):937-945.

[2] 王梁,龚旭,吴伟,陈吉俊,吴冰,李幼华.喷砂对牙科氧化锆陶瓷材料弯曲强度和疲劳性能的影响[J].温州医科大学学报,2017,47(08):585-589.

[3] McLean JW,Hughes TH.The reinforcement of dental porcelain with ceramic oxides. Br Dent J,1965,119( 6) : 251-267.

[4] Della Bona A,Kelly JR.The clinical success of all-ceramic restorations.J Am Dent Assoc,2008,139 ( Suppl) : S8-S13.

[5] 张飙.白榴石对牙科玻璃陶瓷强度的影响.北京口腔医学,1999,7( 1) : 44-47.

[6] Li Cong et al. Interfacial characterization and erosive wear performance of zirconia toughened alumina ceramics particles reinforced high chromium white cast irons composites[J]. Tribology International, 2022, 165.

[7] 周金爱.二氧化锆全瓷技术在口腔修复中的临床应用[J].基层医学论坛,2020,24(08):1102-1103.

[8] 朱海燕.口腔修复材料氧化锆陶瓷的研究与应用[J].世界最新医学信息文摘,2019,19(A5):106-107.

[9] Oonishi H. Jr. et al. EFFECTS OF ROUNDNESS AND ROUGHNESS OF ALUMINA CERAMIC HEAD ON WEAR PROPERTIES FOR LONG -TERM CLINICAL USE[J]. Orthopaedic Proceedings, 2018, 92-B(SI).

[10] 马晴,施丽燕,黄思雪,郑章博文,张爱华,战德松,付佳乐.氧化锆陶瓷在牙体修复领域的研究现状及展望[J].中国组织工程研究,2021,25(22):3597-3602.

[11] 李洪超. 美学氧化锆陶瓷的制备与性能研究[D].湖北工业大学,2020.

[12] Mclean JW, Odont D. Evolution of dental ceramics in the twenties century[J]. J Prosthet Dent, 2001,85:61-69.

[13] Kelly JR,Benetti P.Ceramic materials in dentistry: historical evolution and current practice. Aust Dent J,2011,56 ( Suppl 1) : 84-96.

[14] 杨兆雄. 长石瓷的岩相分析. 硅酸盐通报,1980,( 3) : 51-55.

[15] Bitencourt Sandro Basso et al. Effect of handling material on mechanical and optical properties of feldspathic porcelain.[J]. Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.], 2021, 33(6) : 919-924.

[16] Santos MJ,Costa MD,Rubo JH,et al.Current all-ceramic systems in dentistry: a review.Compend Contin Educ Dent,2015,36( 1) : 31-37.

[17] Wang ChunCheng et al. Comparison of optical and crystal properties of three translucent yttria-stabilized tetragonal zirconia polycrystals with those of lithium disilicate glass-ceramic material.[J]. Journal of dental sciences, 2021, 16(4) : 1247-1254.

[18] Malgaj Tine et al. The Influence of Nanostructured Alumina Coating on Bonding and Optical Properties of Translucent Zirconia Ceramics: In Vitro Evaluation[J]. Coatings, 2021, 11(9) : 1126-1126.

[19] Juntavee Niwut and Juntavee Apa and Plongniras Preeyarat. Effectiveness of Nanohydroxyapatite on Demineralization of Enamel and Cementum Surrounding Margin of Yttria-Stabilized Zirconia Polycrystalline Ceramic Restoration.[J]. TheScientificWorldJournal, 2021, 2021 : 5540738-5540738.

[20] 王 勋,张修银. 全瓷修复体修复后可能出现的问题分析. 口 腔颌面修复学杂志,2008:9(2):148- 151

[21] Sailer I, Feher A, Filser F, et al. Five- year clinical results of zirconia framew orks for posterior fixed partial dentures. Int J Prosth odont, 2007,20:383- 388

[22] Charles R. Dynamic fatigue of glass [J]. Journal of Applied Physics, 1958,29(12):1657-1662.

[23] Evans A, Wiederhorn S. Crack propagation and failure prediction in silicion nitride at elevated temperature [J]. Journal of Materials Science, 1974,9(2):270-278.

[24] Qiao G, Hongjie W, Zhihao J. Comparison between fatigue behavior of some ceramics:a new concept of intrinsic stress-corrosion exponent n0 [J]. International Journal of Fatigue,2002,24(5):499-508.

[25] MAI Y W, ATKINS A G. Crack propagation in ceramic materials under cyclic loading conditions[J]. Metallurgical and Materials Transactions A, 1975, 6(11):2161-2163.

[26] OKAZAKI M, MCEVILY A J, TANAKA T. On the mechanism of fatigue crack growth in silicon nitride[J]. Metallurgical Transactions A (Physical Metallurgy and Materials, Science), 1991, 22(6):1425-1434.

[27] 韩高月. 抛光和上釉对钇稳定型氧化锆循环疲劳性能的影响[D].华北理工大学,2020.DOI:10.27108/d.cnki.ghelu.2020.000394.

[28] 赵海丹, 胡宇平, 张春宝, 何惠明. 牙科氧化锆陶瓷材料循环疲劳性能的实验研究[J]. 牙体牙髓牙周病学杂志, 2013, 23(05):344-348.

[29] 王景坤. 临床调磨对钇稳定型氧化锆循环疲劳性能的影响[D]. 华北理工大学, 2018.

[30] 覃小凤,苏晓晖,欧俊,韦赞军.干湿环境下循环载荷对氧化锆-饰面瓷叠层瓷结构抗弯强度的影响[J].口腔颌面修复学杂志,2010,v.11;No.48(06):324-328.

[31] DAUSKARDT R H, CARTER W C, VEIRS D K, et al. Transient subcritical crack-growth behavior in transformation-toughened ceramics[J]. Acta Metallurgica et Materialia, 1990, 38(11):2327-2336.

[32] KELLY J R, CESAR P F, SCHERRER S S, et al. ADM guidance-ceramics: Fatigue principles and testing[J]. Dental Materials, 2017, 33(11):1192-1204.

[33] LOHBAUER U, ROLAND F, PETSCHELT A, et al. Correlation of in vitro fatigue data and in vivo clinical performance of a glassceramic material[J]. Dental Materials Official Publication of the Academy of Dental Materials, 2008, 24(1):39-44.

引用本文

纪元, 王子健, 潘惠惠, 陈曦, 冯丽芳, 陶瓷类材料的发展和应用概述及疲劳的研究[J]. 国际材料科学通报, 2022; 4: (1) : 1-6.